Self-hardening casting facility, Dissolution facility, Molding facility, Vibration facility, Post processing facility and more
ㆍPipe relationship wear does not happen hardly by(o.5~2m/sec) vulgarity transport that is diffrent from usual mehtod.
ㆍBecause do low speed transfer, sand's particle breakdown does not happen.
ㆍBecause interior air is exhausted by lower part level, sand relationship filling becomes festinately.
ㆍAIR consumption is few than usual method.
Model |
LPC-300 |
LPC-500 |
LPC-1000 |
LPC-1500 |
Capacity (T/Hr) |
5~10 |
10~15 |
15~20 |
20~30 |
Vessel (mm) |
Φ800 |
Φ1000 |
Φ1200 |
Φ1400 |
Flow pipe (mm) |
Φ89 |
Φ114 |
Φ140 |
Φ165 |
Dimension (Φ×H)(mm) |
Φ800×1750 |
Φ1000×2200 |
Φ1200×2600 |