TOP
축전지 제조업체, 축전지설비, 에너지축전시스템, 축전지, 전기용 기계장비
MIXED METAL OXIDE ANODES
Mixed metal oxide anodes have very low consumption rates under 1.0 mg/amp-yr, and can be operated at high current densities in fresh water and in salt water. Because of these impressive performance capabilities, Cathoway sdn.bhd manufactures mixed metal oxide probe anodes for use in heater treaters, condenser water boxes and pressure vessels. The anodes are composed of titanium rods, which are covered with a mixed metal oxide coating. The titanium is inherently resilient and stable, allowing the probe anodes to withstand water turbulence without damage. Because the titanium does not discharge current, electrical current transfer is accomplished through the mixed metal oxide coating. The coating is immune to abrupt current reversals and may be exposed to high current overloads for initial structure polarization without causing harm to the anode.
MMO Tube Anodes
Dimension | Current Output | Life time | |
Diameter | Length | ||
25mm | 1000mm | 8 amp (based on 100amps/㎡) | 20 years |
25mm | 500mm | 4 amp (based on 100amps/㎡) | 20 years |
19mm | 1200mm | 7 amp (based on 100amps/㎡) | 20 years |
23mm | 1200mm | 12 amp (based on 100amps/㎡) | 20 years |
MMO Ribbon Anode
Dimension | Current Output | Life time | ||
Width | Thickness | Length | ||
12.7 mm | 0.6 mm | 152 m | 34 mA/meter(10aA/ft) | 50 years |
Titanium ASTM 265, coated with IrO2/Ta2O5
Magnesium Anodes
Magnesium has the highest driving potential of any sacrificial anode. Magnesium anodes are used for corrosion protection in most direct earth burial applications and in higher resistivity, aqueous electrolytes.
Cathoway Sdn.Bhd. provides a complete range of anode types, high potential and standard one and different dimensions for your cathodic protection system.
High Potential Mg Anodes
Alloy Composition | |
Element | % |
Aluminum (max) | 0.01 |
Manganese (min) | 0.50-1.30 |
Iron (max.) | 0.03 |
Nickel (max.) | 0.001 |
Copper (max.) | 0.02 |
Other (max.) | 0.30 |
Magnesium | Balance |
Typical Electrochemical Properties | |
Amps/h/lb | 500-580 |
Efficiency | 50-58% |
Closed circuit potential | -1.5 to 1 1.75v |
open circuit potential | -1.70 to -1.78v |
High Silicon Cast Iron Tubular & Solid Anodes | |
Element | content % |
Silicon | 14.20-14.75 |
Chromium | 3.25-5.00 |
Managanese | 1.50 max |
Carbon | 0.70-1.10 |
Copper | 0.50 max |
Molybdenum | 0.20 max |
Iron | Remainder |
Anodes can be supplied with cables suited
for the wide range of site conditions
- Kynar / HMWPE
- HMWPE
- XLPE/PVC
- PVC/PVC
The dimensions for the high high silicon iron anodes can be adjusted according to the client requirements.
Test Station
Steel Test Station Data
- Length : 1600mm
- Diameter : 127mm
- wall thickness : 4mm
- Terminals : To suit customer requirement but typically 6 terminals mounted on a non conductive phenolic/PVC board 8mm thick
- Finish : Powder coated paint
- Color : Yellow
Any other requirement can be achieved.